Sedimentation method of spodumene - positive flotation process

Beneficiation flotation spodumene CKS method often used, its essence is finely ground ore, flotation spodumene, sodium hydroxide or sodium carbonate in an alkaline slurry, after high concentration, with vigorous stirring, After multiple times of washing and de-mudging, the fatty acid (such as oleic acid) or its soap is used as a collector to directly float the spodumene: after three selections, the grade is more than 5% Li 2 O, and the recovery rate is obtained. 70% to 75% of spodumene concentrate. A mine ore in Xinjiang contains 1.3% Li 2 O. After normal temperature flotation, the grade of spodumene concentrate is 4% to 5%, and the recovery rate is 85% to 90%.